The Shop => Metal Stuff => Topic started by: bry1975 on June 03, 2011, 08:48:27 PM
-
Any of you chaps had the pleasure of handling or testing Kolsterized 300 series stainless parts?
TIA
Bry
-
Bry - the company I mentioned to you on another subject uses this treatment widely on their SS items. Avoids galling problems on the threads etc.
-
Thanks David,
I actually sent TWO 304 grade dome nuts out to the hardeners last week will be interesting to see how the kolsterising turns out.