Gallery, Projects and General > How do I??
Bonding Acrylic
John Rudd:
MEK= Methyl Ethyl Ketone...
If you can get it...
I got some stuff from a local fab house but it was very pricey.. They were not supposed to sell it direct to the public. Not sure what it was, clear, colourless and no odour...Applied with a syringe to bond..
I mad a perspex cover to go over the belt drive on my mini mill...Even after years of rough handling it survives the use and abuse of the workshop..
Brass_Machine:
I have some MEK. Use it for the epoxy I have for the CF work. hmmm....
Eric
Bluechip:
--- Quote from: John Rudd on March 04, 2013, 03:35:22 AM ---MEK= Methyl Ethyl Ketone...
If you can get it...
I got some stuff from a local fab house but it was very pricey.. They were not supposed to sell it direct to the public. Not sure what it was, clear, colourless and no odour...Applied with a syringe to bond..
I mad a perspex cover to go over the belt drive on my mini mill...Even after years of rough handling it survives the use and abuse of the workshop..
--- End quote ---
MEK ?? Easy enough to buy even now it seems.
http://www.ebay.co.uk/itm/Methyl-Ethyl-Ketone-MEK-1L-can-1-Litre-1000ml-/280930596476?pt=UK_BOI_Medical_Lab_Equipment_Lab_Supplies_ET&hash=item4168c4b67c
Thought the 'Elfins had got at it but apparently not .... er .. yet ??
I used to get it quite easily locally together with acetone in my 'long ago' model boat days ..
Used for glass-fibre ( fiber for the US folk :wave: ) general purpose solvent.
Hmmm glass-fibre .. I remember it well. Webbed fingers, toes , eyelids, bostin' to 'point Percy at the Porcelain' and terrified to go in case I spent the rest of eternity stuck to me wotsit ... :palm: ... made one hull and abandoned the idea ... sloshing about making PCB's is a bit messy but it's got nothing on glass-fibre ..
Dave BC
andyf:
Dave, When using glass fibre, the real problem isn't getting stuck to the distinguishing mark of your sex; it's the itchy fibres on your fingers. At times like that, having a sympathetic partner around the house can be a godsend. If alone, carefully pull down nether garments and sit on the pot like you did as a child.
Ditto if you have been chopping up chillies.
Andy
doubleboost:
It was not the raw matting or the resin that got me .
It was the grinding dust
It gave me "spotty arms" after a few weeks i got used to it :lol: :lol: :lol: :lol: :lol:
We were laminating race car body pannels
John