Bernd:
--- Quote from: 75Plus on October 28, 2009, 05:42:23 PM ---Only disappointment was that it will NOT do the nice colors as is found on some of the better shotguns.
Joe
--- End quote ---
Isn't that called "bluing" and is done with some kind of salts or oils? A kit for bluing, both hot and cold, can be bought from Brownells.
Bernd
75Plus:
--- Quote from: Bernd on December 25, 1973, 09:28:20 AM ---
Isn't that called "bluing" and is done with some kind of salts or oils? A kit for bluing, both hot and cold, can be bought from Brownells.
Bernd
--- End quote ---
I am not referring to bluing Bernd, take a look at this site for an excellent example of color case on a double bbl. shotgun.
http://www.danthegunman.com/index.php?option=com_content&task=view&id=16&Itemid=25
Joe
Joe
Bernd:
Joe,
Thanks for showing that. I'd forgotten about the bone and wood charcoal. Those are nice colors. I bet it takes a bit of practice to get that kind of beauty out of metal.
Bernd
NickG:
Stew, might need to borrow that soon :lol:
:offtopic: How tight do you go with those nuts? Do you have graphited yarn behind them or 'o' rings?
Nick
sbwhart:
High Nick
I used graphite yarn you don't have to go too tight just so you feal a little resistance.