The Shop > Metal Stuff
Milling question.
<< < (3/3)
Stilldrillin:
Thasright! ....... In theory!  :palm:

Drinks can/ cooking foil usually works wonders. Good luck!  :thumbup:

David D
BK:
I did the tramming thingo today, 10 thou out over 10" (on the long thingy  ::)) I put 5 thou under one side, then checked the other way, another 2 thou (shim brass) I can live with what I have now, about .0015" out each way.
Thanks for the advice.
Stilldrillin:
Well done Bernie!  :clap:

That's my first job, for Monday morning......  :thumbup:

David D
Bogstandard:
Sorry I didn't get back to you on the length issue, must have missed it.

There are in fact more reasons to getting the tramming perfect than people realise, and a query from Bernd about why I was machining a part a certain way was explained by this posting.


http://madmodder.net/index.php?topic=2083.msg22206#msg22206


I hope it explains it to you just as well.


John

BK:
It certainly did Bogs, thanks for the link.  :thumbup:
Navigation