awemawson:
I mainly use dry silver sand and sodium silicate Steve - far less messing about and moulds are robust to handle. It also gives a good open mould that breathes with little venting required.

vtsteam:
How is the finish on cast iron?

awemawson:
It's always been pretty good - certainly OK for my stuff and better than green sand by far. I suspect that the hard skin is less as well as there is less chilling effect as no moisture to speak of.

vtsteam:
Post some photos of the out of the mold finish, some time when you're less busy Andrew, I'd like to see that. Maybe you could do a thread on how you cast with pics of the whole process.  :dremel:

vtsteam:
Cylinder casting, poured 3 hours ago, as broken out: