snub:
I have some oil hardening and some water hardening "drill rod" which I believe is the same as silver steel. It is ready for machining but I'm not familiar with the process of hardening. Do I simply get it red hot and then quench it? I thought it would be brittle at this stage and need some further process.
lordedmond:
Ok quick 101

Get it red hot hold it there for about 1 minute per inch thickness test with a magnet while its still red it should now at the correct temp non magnetic , quench in water or oil as per its type w or o

Then rub on some emery cloth to polish the surface , now heat it slowly away from the cutting edge and watch the colour change let it get to straw for a scribe or heat further to blue for a lathe tool then re quench as before.

Stuart
snub:
Thanks for the tutorial, Stuart, but I'm not getting the " Let it go to straw for a scribe". Do I need a translator here? (lol)